Sagging
Symptoms
Localised "drips" and "tears" appear.
Cause
Paint not applied evenly over the surface Coats applied too heavily Paint doesn't have the right consistency (incorrect thinning) Solution
Remove by sanding after thorough drying is completed. Apply the coatings thoroughly and and evenly. Apply at the proper viscosity and the recommended wet film thickness.